cobalt based welding wires
AWS A5.21RCoCr-B stellite 12 mig tig welding wires used in Wood sawtooth,
GB/T 29713 RCoCr-B
YB/T 5092 H112
AWS A5.21 RCoCr-B
ISO 14343-B-RCoCr-B
Description:
ND112 cobalt-based surfacing tig welding wires in the Co-Cr-W surfacing alloy with moderate hardness, wear resistance than ND111 good, but slightly less plastic, with good corrosion resistance, heat and wear resistance, about 650 ℃ high temperature Still maintain these characteristics.
Use:
Mainly used for high temperature, high pressure valves, internal combustion engine valves, high pressure pump sleeve and liner sleeve, hot roll hole type welding
Deposited metal Chemical composition (%)
project (guarantee value):
C 1.2-1.7
Mn ≤1.0
Si 0.4-2.0
Cr 26-32
W 7.0-9.5
Fe 2.0
Co margin
S -
Cu -
Reference current (AC, DC-):
diameter(mm) Welding current(A)
1.6 50~100
2.0 100~200
2.5 200~300
3.2 300~400
Surfacing layer hardness HRC: 45-50
Key attributes:
material: cobalt base alloy
operating temperature: 500-800
welding current: standard
customized support: OEM, ODM, OBM
place of origin: Hebei, China
model number: AWS A5.21 RCoCr-B
brand name: Naidi
application: wood saw tooth, hot rolling finishing roller pass
operating current: standard
warranty: 3year
Product name: AWS A5.21RCoCr-B stellite 12 mig tig welding wire rod
hrc: 45-50
Package: 5KG/PVC BOX 15kg/spool
temperature: 500-800 centidegree
tensile of strenght: 840mpa
Standard: aws ERCOCR-B S112
Feature: good heat and wear resistance
Usages: valves, internal combustion engine valves
OEM: Accept OEM
Shape: mig
Packaging and delivery:
Selling Units: Single item
Single package size: 50X50X30 cm
Single gross weight: 17.000 kg
Lead time:
Quantity 1 - 450 kilograms Lead time 7 days
Quantity > 450 kilograms Lead time To be
Precautions:
1. Protection of gas: the use of pure Ar; flow: current in the 100 ~ 200A 9 ~ 14L / min, the current in the 200 ~ 300A 14 ~ 18L / min.
2. Tungsten pole extension length: 3 ~ 5mm; arc length: 1 ~ 3mm.
3. Wind speed limit of ≤ 1.0m / s; Proposed in the welding area on the back of the argon protection.
4. In the welding, the welding line energy directly affects the size of the weld metal mechanical properties and crack resistance, etc., should be more attention.
5. The welding parts of the rust layer, moisture, oil, dust, etc. in addition to the net.The above recommend ations are for reference only, in the specific operation of the prevailing situation prevail. If necessary, first process evaluation and then determine the welding program.
18831920121